Raman Optical Fiber

Call for Price

Item Number
36736

Description
Raman Optical Fiber


Compare

Description

Item Number
36736

Description
Raman Optical Fiber


Attenuation maximum @ 1450 nm, 0.46, maximum @ 1550 nm, 0.36, typical @ 1450 nm, 0.43, typical @ 1550 nm, 0.33 (dB/km)
Proof Test Level 100 (kpsi)
Proof Test Level 0.689 (GPa)
Typical Applications Discrete Broadband Raman Amplifiers, Raman Lasers
Options The fiber can be delivered on a 29 x 175 mm spool, optionally with standard fiber pigtails spliced to it, and with a layer of protective silicone to protect against mechanical damage.
Type Non-Standard
Cladding Diameter 125 ± 1 (µm)
Coating Diameter 200 ± 15 (µm)
Cutoff Wavelength ≤ 1050 (nm)
Core Eccentricity < 0.6 (µm)
Polarization Mode Dispersion (PMD) (Typical) 0.05 (ps/km0.5)
Polarization Mode Dispersion (PMD) (Maximum) 0.5 (ps/km0.5)
Cladding Non-Circularity < 0.9%
Effective Area @ 1450 nm, 16.1 ± 1.5, @ 1550 nm, 18.7 ± 1.5 (µm2)
PM or non-PM non-PM
Delivery On a 105 x 265 mm spool
Peak Raman Gain Efficiency (typical) 2.5 ((W·km)-1)

Brand